[ 1 ]  [ 2 ]  [ 3 ]  [ 4 ]  [ 5 ]  [ 6 ]  [ 7 ]  [ 8 ]  [ 9 ]  [ 10 ]  [ back ] 


  The calorimeter is built out of lead, plexi and glue [2] which are composed as follows:

The hardener has been simulated as a mixture of several materials which composition is given in Table 1.

Table 1: Composition of hardener mixture [2].

Compound formula fraction
Polyoxypropylediamine C7H20O3 90%
Triethanolamine C6H15O3 7%
Aminoethylpiperazine C6H15N3 1.5%
Diethylenediamine C4H10N2 1.5%